Repository logo
Communities & Collections
All of DSpace
  • English
  • العربية
  • বাংলা
  • Català
  • Čeština
  • Deutsch
  • Ελληνικά
  • Español
  • Suomi
  • Français
  • Gàidhlig
  • हिंदी
  • Magyar
  • Italiano
  • Қазақ
  • Latviešu
  • Nederlands
  • Polski
  • Português
  • Português do Brasil
  • Srpski (lat)
  • Српски
  • Svenska
  • Türkçe
  • Yкраї́нська
  • Tiếng Việt
Log In
New user? Click here to register.Have you forgotten your password?
  1. Home
  2. Browse by Author

Browsing by Author "CHOU, Yu-Lin"

Filter results by typing the first few letters
Now showing 1 - 1 of 1
  • Results Per Page
  • Sort Options
  • No Thumbnail Available
    Item
    聚(丙烯酸/丙烯醯胺)/矽灰複合水膠的合成和性質研究
    (2015) 周佑霖; CHOU, Yu-Lin
    本論文為製備兩種陰離子型的高吸水性水膠,polyacrylic acid/polyacryl amide ( P(AA/AM) )和polyacrylic acid/polyacryl amide/silica fume (P(AA/AM)/SF),起始劑為ammmonium persulfate (APS ),交聯劑為N,N’methylene bisacrylamide (MBA),使用FT-IR作結構鑑定,樣品表面孔洞透過SEM觀察,影響反應的參數包括:單體比例、起始劑劑量、交聯劑劑量、反應溫度和矽灰比例,接著浸泡到純水和鹽水及各種不同環境中測其吸水率。並測試兩種水膠的機械性質,包含抗壓強度。 接著評估P(AA/AM)水膠加到水泥漿和水泥砂漿中作為自養護劑時,添加劑量和是否合宜,於水泥漿中探討其水化程度、圓盤裂縫和凝結時間;水泥砂漿中則探討水分重量損失、保水率、抗壓強度、內部濕度和乾縮量。 實驗結果顯示,在最佳反應條件下,P(AA/AM)/SF水膠在純水中的吸水率為410.5(g/g),0.1M NaCl(aq)和0.1M CaCl2(aq)的吸水率分別為43.4、24.4 (g/g)。抗壓強度為48.6(Kgf/cm2)。 將P(AA/AM)水膠加入水泥砂漿中當自養護劑,最佳劑量為0.2(wt%) 和10(wt%)時,對水泥砂漿及水泥漿中的重量損失、抗壓強度,內部濕度、乾縮量和圓盤裂縫與控制組比較均提升效能。